Lauetstrasse 13 • CH-8112 Otelfingen • Tel +41 (0)44 844’25’50 • Fax +41 (0)44 844’24’92 • info@buehrer-ag.ch  

 

Examples of redone parts

Worn parts from cast steel. Parts coated and polished. Repair of crankshaft

Worn parts from cast steel.

Parts coated with OSU-60L (13% chrome-plated steel) and polished.

Crankshaft repair with flame or electric-arc spraying process.

coated with AlBz Aluminium parts with improved bearing quatity. Coqwheel with hard coating

Right wave covered with masking tape and sand blasted, left finished coated bearings with aluminium bronze (CuAl 8).

Aluminium parts with improved bearing quatity.

Coqwheel with hard coating

example for low electric restistance parts up to 4m and 1.9t can be coated! Crosshead coated with babbitt metal on tin basis

Anodensubporte: Aluminium coated wit copper (Cu) for low electric restistance

Repair of huge wave shaft (wrong cut). Parts up to 4m length and 5t can be coated!

Crosshead from grey cast iron bearing surfaces coated with babbitt metal on tin basis (SnSbCu 7 4).

Hard coating 70HRc Gear shafts Parts coated with rust free steel

Hard coating 70HRc

Gear shafts

Parts coated with AlBz8.

Roll with new coating
newly coated bearing parts robot in coating action

Newly coated bearing parts

Robot in coating action. Automated process for series.

 

Roll with new coating